The anode bag is made of cotton cloth or chemical fiber fabric and is sleeved on the anode to prevent the anode sludge from entering the bag for solution. The anode is impure, or the anode phosphorus content is improper, and the anode bag is damaged, causing the anode film to escape. Clean the anode and titanium basket every half to one month, and replace the damaged anode bag to ensure the plating solution and bath. The anode bag shall be made of acid resistant polyester cloth or polypropylene cloth.
Product Introduction
The density, thickness, specification and pore size of the anode bag have different effects on blocking the convection and diffusion of anode particles, black film mud particles and copper ions. Although the double-layer anode bag can effectively prevent the anode mud from entering the tank solution, it is not conducive to anodic dissolution, and the tank voltage will increase, affecting the adhesion of the phosphorus film. The anode bag shall not be directly attached to the anode surface. Generally, the anode bag shall be packed with a titanium basket.
Product parameters
Nominal rating (μm) |
Initial accuracy (μm) |
Maximum particles(μm) |
discharge of water (L/min) |
1 |
10~20 |
30 |
15 |
3 |
20~30 |
38 |
20 |
5 |
25~40 |
40 |
25 |
10 |
30~50 |
50 |
30 |
20 |
35~60 |
60 |
32 |
30 |
40~70 |
70 |
36 |
50 |
55~80 |
80 |
40 |
75 |
75~105 |
110 |
45 |